ʻO ka moena pulu lōʻihi ma PAN

ʻO ka moena pulu lōʻihi ma PAN

Hāʻawi ka manaʻo ʻo PAN-based rigid composite i ka ikaika maikaʻi, haʻahaʻa haʻahaʻa thermal conductivity, ablation resistance, oxidation resistance, haʻahaʻa hoʻonui coefficient a me ka hana haʻalulu wela maikaʻi. Hoʻohana ʻia ia i nā kapuahi hoʻokahi-crystal, nā kapuahi polycrystalline, pauka m…

ʻIke ʻenehana

WaiwaiʻO ka PAN pan-based hard composite manaʻo
W/m.k0.75-0.85
% Loaʻa ka carbon,%≥99.8
ppm maʻiʻo lehu ppm≤500
g/cm³ mānoanoa nui, g/cm³0.15-0.25
℃ Stablitiy i ka inert (oxidize-free) ambience, ℃2000-2400
℃ Stablitiy i ka oxidizer ambience, ℃280-320